FH40 Shipbuilding steel plate

FH40 Shipbuilding steel plate

The steel for shipbuilding and oil platform---FH40, is the high tensile strength steel.The shipbuilding steel FH40 is the Hull structural steel.We can provide FH40 shipbuilding steel plate price.

E-mail:[email protected]

Online ChatSend your Inquiry

FH40 Shipbuilding steel plate Description

The FH40 steel plate is mainly used for shipbuilding and oil platform, the shipbuilding grade FH40 can be used in the manufacture of the ship's hull structure, whose weight is more then 10000 tons.  Shipbuilding grade FH40  is the high tensile strength steel,  FH40 steel for shipbuilding and oil platform must be good toughness properties, higher strength, strong corrosion-resistance, the processing properties, and welding properties.

FH40 Shipbuilding steel plate specification:
Thickness: 4mm to 260mm,
Width: 1200mm to 4000mm
Length: 3000mm to 18000mm.

FH40 steel plate Chemical Composition %


Grade

C max

Si max

Mn

P max

S max

Als min

Ti max

Cu max

Cr
max

Ni
max

Mo
max

Nb

V

N max

FH40

0.16

0.50

0.90-1.60

0.025

0.025

0.015

0.02

0.35

0.20

0.80

0.08

0.02-0.05

0.05-0.10

0.009

Note: Generally speaking CE will be 0.40%. If the delivery condition is TMPC, the CE will be : ≤ 0.40% (thickness ≤ 50mm). Ceq% =(C+Mn)/6+(Cr+Mo+V)/5+(Ni+Cu)/15.

FH40 steel plate Mechanical Property


Grade

Rm
(MPa)

Re(MPa) min

A% min

Akv/J min

FH40

510-660

390

20

E.T °C

Thickness (mm)

-40

≤ 50

>50-70

>70-100

L

C

L

C

L

C

41

27

-

 Note: In the list , Rm: .tensile strength,Re: Yield strength,A%: elongation, E.T: experimental temperature,L: lengthways, C: crosswise.

 FH40 steel plate Condition Of Delivery


Grade

Fine grains elements

category

The thickness of steel

≤ 12

>12.5-20

>20-25

>25-35

>35-50

>50-100

FH40

Any

Plate/sheet

N,TM,Q&T

-

Profile steel

N(25),TM(25),Q&T(25)

Note: 1. delivery condition: A =Any ; N=Normalized ; CR=Control Rolled ; TM=TMPC, Temperature - deformation control rolling; AR*= Can be hot rolled with the agreement of Classification Society ; CR*=Can be control rolled with the agreement of Classification Society .
2.  The Figure in the ( ) means the sampling volume to do the impact test, the unit is Ton.(-) means without impact test.

 

Send you inquiry